When using zinc plating trivalent blue passivation to produce, what should I do if the passivation film is prone to yellowing?

When using zinc plating trivalent blue passivation to produce, what should I do if the passivation film is prone to yellowing?

Tue Aug 09 09:26:42 CST 2022

    In the production process of the alkaline galvanizing process, sometimes after the product is galvanized, the film is prone to yellowing after zinc plating trivalent blue passivation, which affects the quality of the product and is not accepted by customers. How should it be solved?

    Bigolly Technology made the following analysis based on the field experience and the characteristics of the zinc plating trivalent blue passivation BZ-215 product:

    1. The pH value of the passivation solution is low. The pH is low, and the product passivation speed is relatively fast, and the pH of the passivation solution should be adjusted within the normal range.

    2. The concentration of passivation solution is too high. If the concentration is too high, the passivation speed of the product is relatively fast, and the addition of the original solution should be stopped, part of the passivation solution should be drained, and water should be added to dilute to the normal range.


    3. The product passivation time is too long. If the passivation time is too long, the passivation speed of the product is relatively fast, and the passivation time should be shortened reasonably according to the requirements of the product.

    4. The temperature of the passivation solution is high. The temperature is high, the product passivation speed is relatively fast, and the temperature should be lowered to within the normal range.

    5. The content of iron ions in the passivation solution is high. If the content of iron ions is high, the passivation of the product is easy to turn yellow. Part of the passivation solution should be drained and the original solution should be replenished to control the content of iron ions in the passivation solution.

    Therefore, we need to pay attention to the above five points in the production process of zinc plating trivalent blue passivation, which can effectively avoid the yellowing of the passivation film and reduce the occurrence of failures.If you are interested in zinc plating trivalent blue passivation, please contact Bigolly customer service, you can get free samples and detailed technical information!