When the electroless nickel plating on the workpiece is slow and the salt spray resistance is poor, try this electroless nickel plating solution

When the electroless nickel plating on the workpiece is slow and the salt spray resistance is poor, try this electroless nickel plating solution

Mon Feb 13 10:24:28 CST 2023

    Mr. Zhou in Shanghai is the owner of a processing factory engaged in electroless nickel plating of various mechanical parts.Recently, Mr. Zhou received orders from several customers, requiring that the salt spray resistance of the workpiece coating should reach 96 hours, and that it should be delivered within two days.However, the electroless nickel plating solution used by Mr. Zhou is slow to be plated on the workpiece, and the salt spray resistance of the coating is poor, which can only reach 72 hours, so the workpiece is always complained by customers.So Mr. Zhou wanted to find a electroless nickel plating solution with fast plating and good salt spray resistance.

    One day, Mr. Zhou found Bigolly Technology through online search and consulted engineers about the characteristics of electroless nickel plating solution.After understanding Mr. Zhou's production situation and the performance requirements of the workpiece, the engineer recommended Mr. Zhou to use this electroless nickel plating solution Ni-811.This electroless nickel plating solution is produced with imported raw materials. The bath is stable and the deposition speed is fast, and can be controlled within 10~15 μm/H, and the corrosion resistance of the coating is good, and the neutral salt spray test of the coating is more than 168 hours.After considering, Mr. A decided to buy a small amount and try it.

    Under the guidance of the engineer, Mr. Zhou used this lectroless nickel plating solution.The feedback said that the deposition rate of the workpiece was faster than the previous one, and the workpiece easily passed the salt spray test, and the coating thickness was 15 μ Workpieces below m can easily pass the neutral salt spray test for 96 hours.Half a month later, Mr. Zhou accepted the customer's order again and purchased a batch of electroless nickel plating solution Ni-811.

    Therefore, when the electroless nickel plating on the workpiece is slow and the salt spray resistance is poor, try this electroless nickel plating solution Ni-811.If you are interested in this electroless nickel plating solution, please contact Bigolly customer service for free samples and detailed technical information!