    Mr. Yang is the boss of a electroplating factory in Ningbo, Zhejiang Province, which processes galvanized hardware.Before, Mr. Yang's screws had no problem with the coating after zinc acid plating, but when plating a batch of spring parts, the coating of the workpiece always peeled.Because the coating quality of the workpiece is poor and cannot meet the customer's requirements, Mr. Yang does not want to lose this big customer, so he wants to look for an acid zinc plating brightener that will not peel.

    One day, Mr. Yang found Bigolly Technology by searching for "acid zinc plating brightener manufacturer" on the Internet. After knowing about Bigolly's company in detail, Mr. Yang asked whether there was an acid zinc plating brightener suitable for him.The engineer recommended this acid zinc plating brightener BZ-528 after knowing Mr. Yang's production process and production situation in detail.

    The engineer explained that, because the springs are mostly made of carbon steel, the adhesion of the coating is poor when using ordinary brighteners in the zinc plating process, and the phenomenon of peeling is easy to occur.This acid zinc plating brightener BZ-528 is a new R&D technology, with TBC active ingredients added, to ensure that the workpiece zinc coating is uniform and bright, fast deposition, and small brittleness, which is very suitable for the zinc plating requirements of various low-carbon steel, high carbon steel, carburized steel, and iron castings.After considering, Mr. Yang decided to try this acid zinc plating brightener first.

    Under the guidance of the engineer, Mr. Yang opened a 50 liter small plating tank for multiple tests, and found that the zinc coating of the spring parts was uniform and bright, and the binding force of the coating was good, without peeling.According to this normal production, the defective rate of the workpiece can be greatly reduced, thus effectively reducing the production cost.So Mr. Yang signed a purchase and sales contract with Bigolly.

    Therefore, it is recommended to use this acid zinc plating brightener BZ-528 when the coating of our spring parts is prone to peeling after galvanizing.If you also want to find such an acid zinc plating brightener that will not peel, you can contact the Bigolly customer service for free samples and detailed technical information!