The coating of high phosphorus electroless nickel is very brittle. Try this high phosphorus electroless nickel plating solution

The coating of high phosphorus electroless nickel is very brittle. Try this high phosphorus electroless nickel plating solution

Fri Oct 07 09:17:44 CST 2022

    Mr. Feng from Qingdao, Shandong Province is the boss of an electroless nickel plating factory.Recently, a batch of steel ball valve workpieces produced by Mr. Feng have been coated with 10~15 μ m thick electroless nickel coating, which is very brittle, and always cracks and falls off after bending 180 °.Since Mr. Feng did not want to lose this big customer, he was eager to find a high phosphorus electroless nickel plating solution with small coating brittleness that could meet customer requirements.

    One day, when searching on the Internet, Mr. Feng saw the high phosphorus electroless nickel plating solution Ni-811 of Bigolly Technology, so he understood the characteristics of this solution in detail and asked whether the coating of ball valve workpiece would be brittle after using the solution.、

    After understanding Mr. Feng's production process and the use of liquid medicine, Bigolly engineer explained:This high phosphorus electroless nickel plating solution Ni-811 is made of imported raw materials. The plating solution has good stability. The coating has excellent hardness, wear resistance and corrosion resistance. The salt spray test is more than 168 hours, and the coating has good adhesion and low brittleness. It is very suitable for the use of this kind of ball valve workpiece.After consideration, Mr. Feng decided to purchase a small amount of electroless nickel liquid Ni-811 for trial.

    Under the guidance of the engineer, Mr. Feng used this high phosphorus chemical nickel solution Ni-811 to produce, even if the thickness of the workpiece coating is 20 μ m. After bending for 180 °, there is no crack and falling off.Moreover, the corrosion resistance of the workpiece is more than doubled, which can greatly improve the service life of the workpiece.So Mr. Feng and Billy signed a long-term cooperative purchase and sales contract.

    Therefore, when our workpieces are plated with high phosphorus electroless nickel and the coating is brittle and easy to fall off,try this high phosphorus electroless nickel plating solution Ni-811 to effectively reduce the defective rate of products.If you also want to find such a high phosphorus electroless nickel plating solution with good adhesion and small brittleness, you can contact Bigolly customer service to obtain free samples and detailed technical information!