We are glad to share with you about the results of our work, company news, and give you timely developments and personnel appointment and removal conditions.
Why do copper acid plating layers develop pockmarks? You might initially try to troubleshoot by looking into the acid copper brightener. However, in reality...
In recent years, the application of electroless nickel solution has become increasingly widespread. This is because the electroless nickel layer has high co...
Why does the tin anode experience accelerated dissolution? This is a question raised by many electroplating factories when using tin plating brighteners. In...
Why does the acid copper brightener you use keep causing problems?
Why is it not advisable to increase the temperature of the acid tin plating bath to the highest level, but rather to keep it within a certain range? What ef...
During the application of alkaline zinc plating additives, in order to ensure the quality of the coating, it is essential to strictly follow the process con...
Why do spring components tend to become brittle after undergoing electroplating following electrolytic degreasing?
Why should the anode current density be lower than 2 amperes per square decimeter when using acid tin plating brighteners?
The electroplating factory must consider the issue from the perspective of achieving good economic benefits, and select the appropriate chemical degreasing ...
In order to enhance production efficiency and ensure the quality of the coating, when using the electroless nickel plating solution, we need to properly car...