We are glad to share with you about the results of our work, company news, and give you timely developments and personnel appointment and removal conditions.
To achieve a bluer trivalent chromium blue zinc passivate film color, some parameters in the passivation process need to be carefully adjusted. The followin...
In the production process of using bright nickel plating additives, due to the weak acidity of the plating solution, it is easy to mix nitrate ions and caus...
What should I do if the galvanized trivalent chromium color passivator fails in daily production? How to quickly troubleshoot?
A customer inquired how to reduce the production of black anode sludge when we use acid tin plating brightener?
In the sulfamate nickel plating process, excessive impurities in the plating solution, especially iron impurities, can seriously affect the quality of the f...
Iron impurities are very common in baths using acid zinc plating brighteners and are the most likely to cause failure.Usually, the accumulation of iron impu...
Zinc alloy die casting is easy to blister, which is a problem for many electroplating factories, because it is related to the straight-through rate of elec...